Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 98.0 J/cm² @Temperature -30.0 °C |
466 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |