Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.00 - 10.5 J/cm² | 38.1 - 50.0 ft-lb/in² | Average value: 9.33 J/cm² Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | cond.; ISO 179-1eU |
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | |
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
Unitika CX-2500 PA6, Dry Transparent nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30 Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-5H PA12-GF50 Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSM-40/4 PA666-MD40 Product description: Grilon TSM-40/4 is a special heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 40% mineral filler. Grilon TSM-40/4 has the following important properties.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Charpy Impact Unnotched | 8.00 J/cm² @Temperature 30.0 °C |
38.1 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-4H black 9915 PA*-GF40 Product description: Grivory GV-6H EF natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | cond.; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 2030 PET Resin High mechanical strength, Creep resistant, Low frictionInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 8.00 J/cm² | 38.1 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |