Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East) UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179 |
Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber Description: PA66 with medium viscosity, 50% glass fiber reinforced.Application: For molding parts with very high stiffness at good thermal stability.Information provided by Ter Hell Plastic GMBH... |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-35 S PA6-GF35 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGZ-15 PA666-GF15 Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15 Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® FG70G30HSR3 BK309 Nylon 66
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45 Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
BASF Procom® D 1188 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |