Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -40.0 °C |
24.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -40.0 °C |
24.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 H-GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 HH-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.10 - 18.0 J/cm² | 24.3 - 85.7 ft-lb/in² | Average value: 11.7 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eU |
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179-1 |
Unitika A1025NO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -20.0 °C |
24.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179 |
BASF Ultradur B 4300 G4 High Speed Unc. 20% Glass Filled PBT Ultradur B 4300 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179 |
BASF Nypel® 6030G HS DB BK 5830 30% Glass Filled PA6 (Dry) Description: Nypel® 6030G HS DB BK5830 is a 30% glass fiber reinforced, heat stabilized, black pigmented, injection molding compound based on recycled PA6..Application: Nypel® 6030G HS DB BK5830.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -20.0 °C |
24.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled Daplen KSX65T20 is a 20% mineral filled grade intended for injection molding. Daplen KSX65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSX65T20 offe.. |