Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -40.0 °C |
22.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasalen 3P-H3130B Polypropylene, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7893/GY Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179-1 |
Unitika A3130 PA6, 35% Mineral Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | IS0179 |
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 MZ 315 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179/1eU |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -30.0 °C |
22.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4412 PC Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179 |
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry) Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering .. |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -30.0 °C |
22.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |