Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV-CM 0515 9005/Z Powder-coatable nylon 6.6 for injection molding, 15% ceramic filled Powder-coatable nylon 6.6 for injection molding, with conductive carbon blackInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -40.0 °C |
17.6 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -40.0 °C |
17.6 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL C73 TFGV1530 Nylon 6.6/6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50-3019 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1-7032-B Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Improved heat resistance.Control disks, cams, sliding elem.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -20.0 °C |
17.6 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | ISO 179-1 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | ISO 179/IeU |
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 3.70 J/cm² | 17.6 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 3.70 J/cm² - NB | 17.6 ft-lb/in² - NB | Average value: 6.18 J/cm² Grade Count:6 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -20.0 °C |
17.6 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
Charpy Impact Unnotched | 3.70 J/cm² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |