Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.75 J/cm² | 13.1 ft-lb/in² | ISO 179/1eU |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Charpy Impact Unnotched | 2.75 J/cm² | 13.1 ft-lb/in² | ISO 179 |
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |