Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO 179 |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8382 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Highly dimensionally stable at ele.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO 179 |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-40 PA6-GF40 Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe) Special tough to rigid grade with very good gloss for all types of housings.Data was collected by ISO methods and provided by BASF. |