Polymer Property : Charpy Impact Unnotched = 0.350 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS NOVODUR® P2L-AT ABS, Injection Grade  (discontinued **)
Injection molding grade, very easy flow, antistatic, high stiffness, high gloss.Applications: Telephones, household goods, disk and video housings, office equipment.Information provided by the manuf..
Charpy Impact Unnotched 0.350 J/cm²
1.67 ft-lb/in²
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
Charpy Impact Unnotched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 7595 Phenolic Formaldehyde Resin, Low Coefficient of Friction, Galvanized, Conductive  (di
Phenolic molding compound, inorganically/organically filled, modified with graphite, good heat conductivity, good sliding properties, conductive in electrical properties.Application areas: Bearers f..