Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | 5.0 t | 5.0 t | 1.8 < t ≤ 4.75 mm |
Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed Nominal Composition: Ti-6 Al-4 V Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength .. |
|||
Bend Radius, Minimum | 5.0 t | 5.0 t | t ≤ 1.8 mm |
Kobe Steel KSTI-9 Alpha-Beta Titanium Alloy, ASTM Gr. 35, Annealed (coil, sheets) Nominal Composition: Ti-4.5 Al-2 Mo-1.6 V-0.5 Fe-0.3 Si-0.03 C Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excel.. |
|||
Bend Radius, Minimum | 5.0 t | 5.0 t | 1.8 < t ≤ 4.75 mm |
Kobe Steel KSTI-9 Alpha-Beta Titanium Alloy, ASTM Gr. 35, Annealed (coil, sheets) Nominal Composition: Ti-4.5 Al-2 Mo-1.6 V-0.5 Fe-0.3 Si-0.03 C Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excel.. |
|||
Bend Radius, Minimum | 5.0 t | 5.0 t | Typical; on 0.078 in (2 mm) sheet |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries .. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero.. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265 Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a.. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Bend Radius, Minimum | 5.0 t | 5.0 t | Typical; on 0.078 in (2 mm) sheet |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V-0.1Ru; ASTM Grade 29) Medium To High Strength General-Purpose Alloy. Property data below are typical of Timet® 6-4 ELI (without Ru). The 0.1 Ru ELI variant is used for enhanced corrosion resistance.Data provided by TI.. |
|||
Bend Radius, Minimum | 5.0 - 6.0 t | 5.0 - 6.0 t | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features.. |
|||
Bend Radius, Minimum | 5.0 t | 5.0 t | Typical; on 0.078 in (2 mm) sheet |
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32) High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f.. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A .. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Bend Radius, Minimum | 5.0 t @Thickness 2.00 mm |
5.0 t @Thickness 0.0787 in |
Typical; sheet |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |