Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.60 J/cm² @Temperature 0.000 °C |
31.4 ft-lb/in² @Temperature 32.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |