Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.10 J/cm² @Temperature 23.0 °C |
29.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.10 J/cm² @Temperature 23.0 °C |
29.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu.. |
|||
Charpy Impact, Notched | 6.09 J/cm² @Temperature 22.8 °C |
29.0 ft-lb/in² @Temperature 73.0 °F |
Partial Break; ISO 179 |
ExxonMobil Exxtral™ H1725W Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with very high flow. Product presenting very high rigidity, maintaining excellent impact resistance properties, including at a low tem.. |