Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.600 J/cm² @Thickness 102 mm, Temperature -20.0 °C |
2.86 ft-lb/in² @Thickness 4.00 in, Temperature -4.00 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANTEC PC S60R GF20 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANTEC PC S60R GF30 Polycarbonate, Glass-Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANTEC PC S60R GF30 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV250AF (dry) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K-FHGM24 (Cond.) 30% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(di The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Suzhou Hipro Polymers Hiprolon® 90 NN Nylon 612, condition Hiprolon® 90 NN is medium viscosity polyamide 6.12. Features: low density, low water absorption, high dimension stability, high impact and notched impact resistance, good chemical resistance and .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -20.0 °C |
2.86 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis MG9641B Polyethylene MG9641B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-EH Nylon 66 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® B436 SE PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K225-KS (Cond.) Flame Retardant (Halogen free), Heat Stabilized Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Unipetrol PE HD LITEN® MB/ML 47 HDPE Made for injection molding and special applicationsInformation provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Charpy Impact, Notched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML3286 PC (Europe-Africa-Middle East) LEXAN ML3286 is a 17% glass reinforced grade for use in less demanding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |