Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.460 J/cm² @Temperature 23.0 °C |
2.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature 23.0 °C |
2.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -20.0 °C |
2.19 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -30.0 °C |
2.19 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A ECP3808 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -20.0 °C |
2.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Charpy Impact, Notched | 0.460 J/cm² @Temperature -20.0 °C |
2.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |