Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 26.3 J/cm² @Temperature 704 °C, Time 3.60e+6 sec |
125 ft-lb/in² @Temperature 1300 °F, Time 1000 hour |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |