Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to.. |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
SABIC P6006 Black High Density Polyethylene for Pipes Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Charpy Impact, Notched | 2.60 J/cm² @Thickness 102 mm, Temperature -20.0 °C |
12.4 ft-lb/in² @Thickness 4.00 in, Temperature -4.00 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical NT-520 ABS, High Flow, Non Toxic Information Provided by LG Chem |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BTE30-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 0.000 °C |
12.4 ft-lb/in² @Temperature 32.0 °F |
ISO R179 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Akulon® K224-G8 PA6-GF40 40% Glass Reinforced |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1017GH33 BK701 PA6-GF33 33% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact, Notched | 2.60 J/cm² @Temperature -30.0 °C |
12.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |