Charpy Impact, Notched 0.340 J/cm²

@Temperature 23.0 °C
1.62 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A CP400 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.340 J/cm²

@Temperature -30.0 °C
1.62 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® S650FR BK851 PBT  (Unverified Data**)
Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.340 J/cm²

@Temperature -30.0 °C
1.62 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Solvay TECHNYL® C 52G1 V20 PA6, Conditioned
Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer..
Charpy Impact, Notched 0.340 J/cm²

@Temperature 23.0 °C
1.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
Charpy Impact, Notched 0.340 J/cm²

@Temperature -30.0 °C
1.62 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Charpy Impact, Notched 0.340 J/cm²

@Temperature 23.0 °C
1.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..