Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.130 J/cm² @Temperature -20.0 °C |
0.619 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PH 52 T 20 003/1M Polypropylene reinforced with 20% mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Charpy Impact, Notched | 0.130 - 0.200 J/cm² @Temperature 23.0 °C |
0.619 - 0.952 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Charpy Impact, Notched | 0.130 - 0.200 J/cm² @Temperature 23.0 °C |
0.619 - 0.952 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group MELOPLAS® 182 MF Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf.. |
|||
Charpy Impact, Notched | 0.130 - 0.200 J/cm² @Temperature 23.0 °C |
0.619 - 0.952 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature -20.0 °C |
0.619 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature -20.0 °C |
0.619 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-1120 AN is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1120 AN is develo.. |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature 23.0 °C |
0.619 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® BB 85 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature 23.0 °C |
0.619 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® FB 85 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature -20.0 °C |
0.619 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature -20.0 °C |
0.619 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature -20.0 °C |
0.619 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |