Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Europe-Africa-Middle East) Improved flow PC with excellent processability and mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD124R PC (Europe-Africa-Middle East) LEXAN FXD124R is a transparent/translucent low viscosity grade for light diffusion special effects. FDA compliant. Color package may affect performance.This data was supplied by SABIC-IP for the Eu.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East) Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE123R PC (Europe-Africa-Middle East) LEXAN FXE123R is a transparent/translucent, UV stabilised low viscosity grade for special effects colors with a fluorescent appearance. Color package may affect performance.This data was supplied by.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LR180 PC (Europe-Africa-Middle East) LR180 is a medium viscosity, non UV, non release containing multipurpose polycarbonate recycle gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® Fuel Lock FL-LP PA6 Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized |
|||
Charpy Impact, Notched | 6.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
30.9 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |