Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.60 J/cm² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3).. |
|||
Charpy Impact, Notched | 4.60 J/cm² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Charpy Impact, Notched | 4.60 J/cm² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |