Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East) C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 65CI PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
19.0 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A53^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANBLEND FS7 FR UV PC/ASA Blend, Flame-Retardant, UV Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANTEC PC S60R Polycarbonate Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANTEC PC S75R Polycarbonate Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-P2 Impact Modified Nylon 66 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-5000 Polypropylene Block-Copolymer INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automot.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 506 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179-1eA |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East) XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |