Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A USZ200 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 0.000 °C |
57.1 ft-lb/in² @Temperature 32.0 °F |
Injection Molded; ISO 75-2/B |
Braskem INSPIRE™ 137 NA Performance Polypropylene Polymer INSPIRE™ 137 Performance polymer is an impact copolymer, primarily designed for film extrusion and suitable for blow molding where high mechanical properties are of the highest importance.INSPIRE 1.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
DIN EN ISO 179 |
BASF Elastollan 1185 A FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |