Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs V0E ABS, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.80 J/cm² @Thickness 102 mm, Temperature -20.0 °C |
8.57 ft-lb/in² @Thickness 4.00 in, Temperature -4.00 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV300 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Lanxess Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, low viscosity, good flowability (Easy Flow), good heat-resistanceApplication Examples: gearbox housings, spring holders, automotive door handles |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
Injection Molded; ISO 179/1eA |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East) NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl PKN4736 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4736 is a PPO+HIPS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulations.This .. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Akulon® Fuel Lock FL-LP PA6 Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® K224-G8 PA6-GF40 40% Glass Reinforced |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HG7 (Dry) 35% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-PG8 (Dry) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
8.57 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |