Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 0.000 °C |
8.09 ft-lb/in² @Temperature 32.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S RV500 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs F00 ABS Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-PG2U (Dry) 13% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -40.0 °C |
8.09 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers PA 66, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BTG30-FN03N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -20.0 °C |
8.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
Styron Magnumâ„¢ 3525 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3525 is a resin with excellent processing characteristics. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with a stable.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 236F4Q32 Nylon 6.6, 20% Glass Fiber SAXAMID 236 F4Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers and very good flow properties. It is suitable for applications requiring toughness in co.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, Conditioned Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |