Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV300AF (cond.) Nylon 66-30GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV150 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S RV200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RCP3010LK (cond.) Nylon 6 PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RCV3015 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
|
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -20.0 °C |
4.04 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polyram RamSter PF305G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -20.0 °C |
4.04 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -20.0 °C |
4.05 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® EB 501 Polypropylene Impact Copolymer Made for extrusion applications. LHTA stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® N2640 E4 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CF350 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV330 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature -30.0 °C |
4.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
Charpy Impact, Notched | 0.850 J/cm² @Temperature 23.0 °C |
4.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |