Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV250FR (dry) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CV300LK (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A CP300K (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HG2U (Dry) 10% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3120 20% Talc Filled Polypropylene Block-Copolymer INNOPOL® CS 2-3120 is a 20% talc filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-3120 is developed for producing.. |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66 Description: Ultramid N-276 BK ND3007 is a 40% mineral/glass reinforced, heat stabilized injection molding PA6/6.Information provided by BASF |
|||
Charpy Impact, Notched | 0.380 J/cm² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |