Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 32 B PA6 Basic type PA 6 for compounding, for general use. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electrical purposes. Excellent flow of the material predetermines it for.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 G 5 Polyamide 6, 5% Graphite FeaturesPA 6 for injection moulding with addition of 5% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, slid.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 G 5 Polyamide 6, 5% Graphite FeaturesPA 6 for injection moulding with addition of 5% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, slid.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 W 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for grips of electric hand tools, hobby tools, gear wheels, covers of electric tools, flat products, automobile wheel .. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP EIP12030F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T15020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | >= 0.300 J/cm² @Temperature -23.0 °C |
>= 1.43 ft-lb/in² @Temperature -9.40 °F |
edgewise; ISO 179 |
MTM Plastics Purpolen® PP Polypropylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Styrolution Luran® S 757 G UV White 37019 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Styrolution Luran® S 757 R Colored ASA Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-LGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-HM8 (Cond.) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 LI LS PA6, improved strength, light stability FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C |
1.43 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |