Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT B 27 PA6 Basic type PA 6 for compounding, for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInformation Prov.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT B 27 PA6 Basic type PA 6 for compounding, for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInformation Prov.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 26 B PA6 Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Information Prov.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 26 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 29 B PA6 Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivered in the natu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT SD PA6 Basic type PA 6 for compounding, modified for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInforma.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 32 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 FRC 2 PA66, basic type FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and co.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 FRC 3 PA 66 basic type with flame retardant Features: Modified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and .. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T15040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² @Temperature 23.0 °C |
0.714 - 1.19 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -40.0 °C |
0.714 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Polykemi AB POLYfill PP HIP8040 VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -40.0 °C |
0.714 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH S4030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3140 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-3140 is a 40% talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3140 is recommended especially for producin.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3120 BPLU 9H0017 is a 20% talc filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3120 BPLU 9H0017 is developed for producing injection molded au.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 812 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 82 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GB 20 PA6 reinforced with 20% glass beads Features: Nearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical proper.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |