Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 3.86 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched >= 2.06 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
>= 3.86 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
3.86 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Porene KU200 Acrylonitrile Butadiene Styrene
Applications:extrusion applicationautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm
3.86 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced
Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 3.17 mm
3.86 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm
3.86 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® HG-0760AT ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 3.17 mm
3.86 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm
3.86 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced
Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 3.17 mm
3.86 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm
3.86 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced
Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm
3.86 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® HG-0760AT ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 3.17 mm
3.86 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 3.17 mm
3.86 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® WR-9120 J ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 6.35 mm
3.86 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced
Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Thickness 3.17 mm
3.86 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® WR-9120 J ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.06 J/cm
<br>@Temperature 23.0 °C
3.86 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H2001WC High Density Polyethylene Wire & Cable Grade
Key Characteristics:Excellent environmental stress cracking resistance (ESCR), high mechanical properties, high speed extrusionRecommended Applications:Jacketing of fiber optical cablesJacketing of ..
Izod Impact, Notched 2.06 J/cm
<br>@Temperature 23.0 °C
3.86 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
Denka MALECCA K-095 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Izod Impact, Notched 2.06 J/cm
3.86 ft-lb/in
Wet; ASTM D256
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66
43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi..
Copyright © lookpolymers.com All Rights Reserved