| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
1.67
J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.12
ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical LUMID HI1102A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.12 ft-lb/in | DIN 53453; ASTM D256 |
|
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | ASTM D256 |
|
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin
G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
3.12
ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
|
IRPC Polimaxx Porene AN450 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectric/electonic housing for microwave oven, tv, vcr, computer, etc.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
3.12
ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
|
IRPC Polimaxx Porene GA400 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectrical applianceselectrical fansair conditionersfloppy disks
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | |
|
Kuraray SEPTON® CM1 Compatibilizer
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
|
|||
| Izod Impact, Notched |
1.67
J/cm @Temperature -30.0 °C |
3.13
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Temperature -30.0 °C |
3.13
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Temperature -30.0 °C |
3.13
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Temperature -30.0 °C |
3.13
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Temperature -30.0 °C |
3.13
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Temperature -30.0 °C |
3.13
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.12 ft-lb/in | |
|
Shinil Chemical SHINSTAT PETG Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.12 ft-lb/in | |
|
Shinil Chemical SHINSTRA PA-66 Devlop Structural Polymer Window Strip
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC
LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Thickness 3.17 mm |
3.12
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Infino® LS-3302 PC, 30% Glass Filled High Impact
High-impact resistant PC/GF with 30% GF reinforcement for camera body tubeInformation provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Thickness 3.17 mm |
3.12
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Thickness 3.17 mm |
3.12
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Infino® LS-3302 PC, 30% Glass Filled High Impact
High-impact resistant PC/GF with 30% GF reinforcement for camera body tubeInformation provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
1.67
J/cm @Thickness 3.17 mm |
3.12
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.13 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL PX2734 PPE+HIPS (Asia Pacific)
PPE/HIPS, unfilled, FR-V1
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.12 ft-lb/in | ASTM D256 |
|
E-Polymers TEKAMID® JN2 PPE+PA66 Un-reinforced Chemical resistance PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
|
|||
| Izod Impact, Notched | 1.67 J/cm | 3.12 ft-lb/in | DIN 53453; ASTM D256 |
|
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric..
|
|||