| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.812 J/cm | 1.52 ft-lb/in | ASTM D256 |
| Omni Plastics OmniTech™ ABS GR20 UV FD BK118, GY695 Flame Retardant UL Approved MaterialOmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, .. |
|||
| Izod Impact, Notched | 0.812 J/cm | 1.52 ft-lb/in | ASTM D256 |
| Omni Plastics OmniTech™ ABS GRC20 NA Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b.. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP KI001XXJ Acetal LNP* LUBRICOMP* KI001XXJ is a compound based on Acetal containing 2% Silicone. Added features of this grade include: Wear Resistant, Healthcare. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL GTX CRN720V PPE+PA6 (Asia Pacific) GF20% FR-GTX, Restricted to sell for new customers |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | |
| Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
| Izod Impact, Notched | 0.814 J/cm | 1.52 ft-lb/in | ASTM D256 |
| E-Polymers TEKAMID® JN910 PPE+PA66 10% Glass Fiber Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
| SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |
|||