| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific)
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific)
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific)
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched |
0.810
J/cm @Temperature -30.0 °C |
1.52
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **)
PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b..
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KI001XXJ Acetal
LNP* LUBRICOMP* KI001XXJ is a compound based on Acetal containing 2% Silicone. Added features of this grade include: Wear Resistant, Healthcare.
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON DEF42 PC
LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON DEP42E PC
LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear..
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific)
LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding.
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific)
LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & ..
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI
LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding.
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL GTX CRN720V PPE+PA6 (Asia Pacific)
GF20% FR-GTX, Restricted to sell for new customers
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | |
|
Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced
Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo..
|
|||
| Izod Impact, Notched | 0.810 J/cm | 1.52 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
|
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP
SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410
|
|||