Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.267 - 4.27 J/cm | 0.500 - 8.00 ft-lb/in | Average value: 0.725 J/cm Grade Count:71 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Izod Impact, Notched | 1.55 - 4.27 J/cm | 2.90 - 8.00 ft-lb/in | Average value: 2.82 J/cm Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 1.07 - 4.27 J/cm | 2.00 - 8.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Izod Impact, Notched | 1.07 - 4.27 J/cm | 2.00 - 8.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Izod Impact, Notched | 1.07 - 4.27 J/cm | 2.00 - 8.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Izod Impact, Notched | 3.74 - 4.27 J/cm | 7.00 - 8.00 ft-lb/in | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Izod Impact, Notched | 3.20 - 4.27 J/cm | 6.00 - 8.00 ft-lb/in | |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Izod Impact, Notched | 1.60 - 4.27 J/cm | 3.00 - 8.00 ft-lb/in | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Izod Impact, Notched | 3.20 - 4.27 J/cm | 6.00 - 8.00 ft-lb/in | |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Izod Impact, Notched | 1.07 - 4.27 J/cm | 2.00 - 8.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Izod Impact, Notched | 1.07 - 4.27 J/cm | 2.00 - 8.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |