Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 - 3.74 J/cm | 1.00 - 7.00 ft-lb/in | Average value: 1.60 J/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 0.267 - 3.74 J/cm | 0.500 - 7.00 ft-lb/in | Average value: 1.14 J/cm Grade Count:57 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | ASTM D256 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Izod Impact, Notched | 2.14 - 3.74 J/cm | 4.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC T14 General Purpose Molding Compound BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Izod Impact, Notched | 1.07 - 3.74 J/cm | 2.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres.. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts... |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Izod Impact, Notched | 0.267 - 3.74 J/cm | 0.500 - 7.00 ft-lb/in | Average value: 0.740 J/cm Grade Count:95 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |