Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.440 - 3.20 J/cm @Temperature -50.0 - 0.000 °C |
0.824 - 5.99 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 1.44 J/cm Grade Count:19 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched | 0.0700 - 3.20 J/cm | 0.131 - 5.99 ft-lb/in | Average value: 0.866 J/cm Grade Count:73 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Izod Impact, Notched | 0.530 - 3.20 J/cm | 0.993 - 5.99 ft-lb/in | Average value: 1.39 J/cm Grade Count:12 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |