Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.86865 - 2.6695 J/cm @Temperature -40.0 - -17.8 °C |
3.50075 - 5.0011 ft-lb/in @Temperature -40.0 - 0.000 °F |
Average value: 2.22 J/cm Grade Count:2 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.80085 - 2.6695 J/cm @Temperature -29.0 - -28.9 °C |
1.5003 - 5.0011 ft-lb/in @Temperature -20.2 - -20.0 °F |
Average value: 1.43 J/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.5339 - 2.6695 J/cm @Temperature -40.0 - 72.8 °C |
1.000 - 5.0011 ft-lb/in @Temperature -40.0 - 163 °F |
Average value: 1.51 J/cm Grade Count:18 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.5339 - 2.6695 J/cm @Thickness 3.17 - 3.17 mm |
1.000 - 5.0011 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.51 J/cm Grade Count:18 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.5339 - 2.6695 J/cm @Temperature -40.0 - -40.0 °C |
1.000 - 5.0011 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.29 J/cm Grade Count:16 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.5339 - 2.6695 J/cm @Thickness 3.17 - 3.17 mm |
1.000 - 5.0011 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.29 J/cm Grade Count:16 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |