Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.588 - 2.50 J/cm | 1.10 - 4.68 ft-lb/in | Average value: 1.38 J/cm Grade Count:5 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Izod Impact, Notched | 0.5339 - 2.50 J/cm @Temperature -40.0 - 0.000 °C |
1.000 - 4.68 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 1.05 J/cm Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 0.5339 - 2.50 J/cm @Thickness 3.17 - 6.35 mm |
1.000 - 4.68 ft-lb/in @Thickness 0.125 - 0.250 in |
Average value: 1.05 J/cm Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 1.50 - 2.50 J/cm @Thickness 4.00 mm |
2.81 - 4.68 ft-lb/in @Thickness 0.157 in |
ASTM D256 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Izod Impact, Notched | 1.50 - 2.50 J/cm @Thickness 4.00 mm |
2.81 - 4.68 ft-lb/in @Thickness 0.157 in |
ASTM D256 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |