Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.37373 - 1.81526 J/cm @Temperature -40.0 - -40.0 °C |
0.70015 - 3.40073 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.08 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Notched | 0.260 - 1.81526 J/cm @Temperature -50.0 - -17.8 °C |
0.487 - 3.40073 ft-lb/in @Temperature -58.0 - 0.000 °F |
Average value: 0.562 J/cm Grade Count:19 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.69407 - 1.81526 J/cm @Temperature -40.0 - 0.000 °C |
1.3003 - 3.40073 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 1.11 J/cm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Izod Impact, Notched | 0.69407 - 1.81526 J/cm @Thickness 3.17 - 3.20 mm |
1.3003 - 3.40073 ft-lb/in @Thickness 0.125 - 0.126 in |
Average value: 1.11 J/cm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |