Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.641 - 7.85 J/cm | 1.20 - 14.7 ft-lb/in | Average value: 2.42 J/cm Grade Count:11 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Izod Impact, Notched | 6.78 - 7.85 J/cm | 12.7 - 14.7 ft-lb/in | |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |