Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.42712 - 7.68816 J/cm @Temperature -40.0 - -18.0 °C |
0.80017 - 14.4031 ft-lb/in @Temperature -40.0 - -0.400 °F |
Average value: 1.66 J/cm Grade Count:31 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 7.21 - 7.68816 J/cm @Temperature -51.1 - 149 °C |
13.5 - 14.4031 ft-lb/in @Temperature -60.0 - 300 °F |
Average value: 7.51 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |