Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.196133 - 0.85424 J/cm @Temperature -30.0 - -18.0 °C |
0.367438 - 1.6003 ft-lb/in @Temperature -22.0 - -0.400 °F |
Average value: 0.562 J/cm Grade Count:9 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.196133 - 0.85424 J/cm @Thickness 3.17 - 6.50 mm |
0.367438 - 1.6003 ft-lb/in @Thickness 0.125 - 0.256 in |
Average value: 0.562 J/cm Grade Count:9 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.26695 - 0.85424 J/cm @Diameter 6.35 - 6.35 mm |
0.50011 - 1.6003 ft-lb/in @Diameter 0.250 - 0.250 in |
Average value: 0.463 J/cm Grade Count:6 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.26695 - 0.85424 J/cm @Temperature 0.000 - 0.000 °C |
0.50011 - 1.6003 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.463 J/cm Grade Count:6 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.85424 - 0.85424 J/cm @Temperature -30.0 - -30.0 °C |
1.6003 - 1.6003 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.854 J/cm Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |