Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.550 - 0.550 J/cm @Temperature -30.0 - -30.0 °C |
1.03 - 1.03 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.550 J/cm Grade Count:1 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini.. |
|||
Izod Impact, Notched | 0.37373 - 0.550 J/cm @Temperature -40.0 - 82.2 °C |
0.70015 - 1.03 ft-lb/in @Temperature -40.0 - 180 °F |
Average value: 0.459 J/cm Grade Count:3 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Izod Impact, Notched | 0.500 - 0.550 J/cm @Temperature -40.0 - -20.0 °C |
0.937 - 1.03 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.642 J/cm Grade Count:1 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched | 0.500 - 0.550 J/cm | 0.937 - 1.03 ft-lb/in | ASTM D256 |
Loxim 230 01V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.150 - 0.550 J/cm @Temperature -20.0 - 0.000 °C |
0.281 - 1.03 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 0.329 J/cm Grade Count:17 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |