Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.5339 - 0.5339 J/cm @Temperature -40.0 - -40.0 °C |
1.000 - 1.000 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.534 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Izod Impact, Notched | 0.5339 - 0.5339 J/cm @Thickness 3.17 - 3.17 mm |
1.000 - 1.000 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.534 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Izod Impact, Notched | 0.400 - 0.5339 J/cm @Temperature -40.0 - -20.0 °C |
0.749 - 1.000 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.445 J/cm Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched | 0.5339 - 0.5339 J/cm @Temperature -28.9 - -28.9 °C |
1.000 - 1.000 ft-lb/in @Temperature -20.0 - -20.0 °F |
Average value: 0.533 J/cm Grade Count:1 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Izod Impact, Notched | 0.5339 - 0.5339 J/cm @Thickness 3.17 - 3.17 mm |
1.000 - 1.000 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.533 J/cm Grade Count:1 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Izod Impact, Notched | 0.5339 - 0.5339 J/cm @Temperature -28.9 - -28.9 °C |
1.000 - 1.000 ft-lb/in @Temperature -20.0 - -20.0 °F |
Average value: 1.55 J/cm Grade Count:1 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Izod Impact, Notched | 0.5339 - 0.5339 J/cm @Thickness 3.17 - 3.17 mm |
1.000 - 1.000 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.55 J/cm Grade Count:1 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |