Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.490332 - 0.490332 J/cm @Temperature 3.20 - 3.20 °C |
0.918594 - 0.918594 ft-lb/in @Temperature 37.8 - 37.8 °F |
Average value: 0.427 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.490332 - 0.490332 J/cm @Thickness 23.0 - 23.0 mm |
0.918594 - 0.918594 ft-lb/in @Thickness 0.906 - 0.906 in |
Average value: 0.427 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.392266 - 0.490332 J/cm @Temperature -30.0 - -30.0 °C |
0.734875 - 0.918594 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.468 J/cm Grade Count:5 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.392266 - 0.490332 J/cm @Thickness 3.20 - 6.40 mm |
0.734875 - 0.918594 ft-lb/in @Thickness 0.126 - 0.252 in |
Average value: 0.468 J/cm Grade Count:5 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |