Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.210 - 0.400 J/cm | 0.393 - 0.749 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.210 - 0.400 J/cm | 0.393 - 0.749 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8530_Gray60 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.350 - 0.400 J/cm | 0.656 - 0.749 ft-lb/in | ASTM D256 |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Izod Impact, Notched | 0.350 - 0.400 J/cm | 0.656 - 0.749 ft-lb/in | ASTM D256 |
Loxim 200 00HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.350 - 0.400 J/cm | 0.656 - 0.749 ft-lb/in | ASTM D256 |
Loxim 315 02HB Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 800 00 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 820 02C HB Polypropylene Compound, 20% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 820 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Izod Impact, Notched | 0.220 - 0.400 J/cm | 0.412 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Izod Impact, Notched | 0.37373 - 0.400 J/cm @Temperature -40.0 - -40.0 °C |
0.70015 - 0.749 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.391 J/cm Grade Count:3 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |