Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | |
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -30.0 °C |
8.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 A |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 A |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D-256 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
KYDEX® V103 High Impact Fire-Rated Thermoforming Sheet Features:Formulated to substitute for FR-ABS sheetVery good impact resistanceEasy to form with excellent part definition and deep-draw characteristicsSuggested Applications:Equipment HousingsExhibit.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled Conductive Carbon, Powder Modified |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R71/920 PC/ABS Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC IM FR Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D 256A |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 7600B (ELG) Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ASAPC GLY 130 UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall CL-6400 Rigid PVC, Molding Georgia Gulf CL-6400 is a high flow clear PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information p.. |
|||
Izod Impact, Notched | >= 4.27 J/cm | >= 8.00 ft-lb/in | ASTM D256 |
Buckeye Polymers BP REPLEX 0805 R BLK ABS Polymer Product Information: Our BP REPLEX 0805 R BLK offers better than average impact while providing good melt flow characteristics in an affordably priced material.Product Features:Good impact and melt .. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 22.8 °C |
8.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D648 |
PolyOne Edgetek® UR-30GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 30% Glass Fiber Reinforced
(di Information provided by PolyOne™ Corporation |