Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.22 J/cm @Temperature -30.0 °C |
7.90 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Ovation Polymers Opnyl OP66UT119 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 3.17 mm |
7.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HI-1001BG PC/ABS, Metal Plating Grade PC/ABS material that can be used in automobile wheel cap and air-conditioner panelInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 3.17 mm |
7.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9700S ASA, Unreinforced Used in golf cart roof etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 3.17 mm |
7.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HI-1001BG PC/ABS, Metal Plating Grade PC/ABS material that can be used in automobile wheel cap and air-conditioner panelInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 3.17 mm |
7.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9700S ASA, Unreinforced Used in golf cart roof etc.Information provided by Samsung Cheil Industries. |