Polymer Property : Izod Impact, Notched = 7.87 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.20 J/cm

@Temperature -40.0 °C
7.87 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Izod Impact, Notched 4.20 J/cm
7.87 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 4.20 J/cm
7.87 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 4.20 J/cm
7.87 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 4.20 J/cm
7.87 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 4.20 J/cm
7.87 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 4.20 J/cm
7.87 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.