Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 4.00 J/cm @Temperature 23.0 °C |
7.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 4.00 - 5340 J/cm | 7.50 - 10000 ft-lb/in | Average value: 13.0 J/cm Grade Count:29 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R26 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 310 Utility Black PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 330 White PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 380 Grey PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | -20°F; ASTM D256 |
Styron Pulse® 2200BG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | LAB034 |
ExxonMobil Mytex™ AS65KW-1ATM Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
7.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 7500E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
7.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 7502 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
7.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.00 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
7.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C40L1 Calcium Reinforced |