Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.75 J/cm | 7.03 ft-lb/in | ASTM D256 |
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co.. |
|||
Izod Impact, Notched | 3.75 J/cm | 7.03 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Izod Impact, Notched | 3.75 J/cm | 7.03 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Izod Impact, Notched | 3.75 J/cm | 7.03 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Izod Impact, Notched | 3.75 J/cm | 7.03 ft-lb/in | ASTM D256 |
Ineos K46-06-185 HDPE K46-06-185 is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, par.. |